Suggestions on reducing tool wear in machining process 2021-07-02


Recommendations for minimizing wear in the tools
Highly glass-loaded thermoplastics can cause significant wear on tools and equipment.
Fiberglass has a Mohs hardness of 7.
Where possible machine parts and tools that are exposed to Polytron should be hardened.
Further, molds should be polished to a 0.0001 (or better) finish
High wear is often seen at the gates. If possible; a hardened insert can help in this high wear area
For long production molds, a Rockwell hardness of +60 is recommended. This can be obtained by using
D2 or A2 steel andthen hardening.
Shorter runs can be effectively managed by placing the molds with electroless nickel, slow deposition
dense chrome or Nye-carb plating
Different long fiber enhance polymer has the same process,but the specific needs also to the actual production process encountered in the specific analysis and solution


Injection mold glass fiber LFT pellets


newsletter

-- get updates with latest topics

Copyright © 2015-2024 Xiamen LFT composite plastic Co.,ltd..All Rights Reserved.

Home

Products

News

contact